VESTAKEEP® 5000G by Evonik is an unreinforced, semi-crystalline, high viscosity polyetheretherketone (PEEK) grade. Exhibits excellent thermal- and chemical resistance. Used for automotive, aerospace, rail cars, machinery and construction apparatus.
- It is a non-combustible, recyclable and self-extinguishing grade.
- It is processed by injection molding and extrusion.
- Recommended for electrical, cable, electronics, semiconductors and medical applications.
- VESTAKEEP® 5000G by Evonik complies with EU (10/2011) and FDA regulation 21 CFR, § 177.2415.
Product family:
Chemical family:
Product Type:
| CAS Number | Visible After Login |
| Bio Based content | Visible After Login |
| Appearance | Visible After Login |
Compliance
| Food Contact Approval | Visible After Login |
| Certifications & Compliance | Visible After Login |
Applications
Recommended markets
Applications
Conversion mode
Availability
Product Status:Visible After Login
VESTAKEEP® 5000G properties
Electrical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Comparative Tracking Index (CTI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dielectric Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Surface Resistance | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Volume Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame Rating, UL 94 | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Flammability Index (GWFI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Ignition Temperature (GWIT) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Dielectric Constant | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dielectric Constant | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Transverse | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Volume Flow Rate (MVR) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| CTE, Linear, Parallel to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melting Point | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
VESTAKEEP® 5000G Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Back Pressure | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Hooper Temperature | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Moisture Content | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Screw Rotation Speed | Visible After Login | Visible After Login | |
| Vent Depth | Visible After Login | Visible After Login | |









