AvaSpire® AV-621 NT is an unreinforced, beige colored, flame retardant polyaryletherketones (PAEK) grade. Is suitable for processing by compression molding, injection blow molding, machining, thermoforming and profile-, fiber (spinning)-, film-, wire & cable- and blow molding extrusion. Offers good chemical resistance, high heat resistance, good ductility, fatigue resistance, good dimensional stability, excellent colorability, good impact resistance and good part aesthetics. Shows better ductility, low melt flow and higher HDT than comparable PEEK grades. Exhibits 20% higher tensile elongation at yield and twice the tensile elongation at break value when compared to PEEK grades. AvaSpire® AV-621 is easily fabricated using conventional thermoplastic melt processing techniques and standard equipment. Used in healthcare/medical applications, transportation, semiconductor, electronics, bearings, bushings, connectors, oil and gas industry and chemical processing. Complies with RoHS.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Appearance | Visible After Login |
Compliance
| Certifications & Compliance | Visible After Login |
Applications
Recommended markets
Applications
Conversion mode
Availability
Product Status:Visible After Login
Regional Availability:Visible After Login| Visible After Login| Visible After Login
AvaSpire® AV-621 NT properties
Electrical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Dielectric Constant | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dielectric Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dissipation Factor | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Surface Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Volume Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame rating (UL 94) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flame rating (UL 94) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Limiting Oxygen Index (LOI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Compressive Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Rockwell | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Poisson ratio | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Shear Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Viscosity, Melt | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Transverse | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Specific Gravity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| CTE, Linear, Parallel to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glass Transition Temperature (Tg) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Heat Deflection Temperature (HDT), Annealed | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melting Point | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Specific Heat Capacity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Specific Heat Capacity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Thermal Conductivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
AvaSpire® AV-621 NT Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Front Temperature | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Middle Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Rear Temperature | Visible After Login | Visible After Login | |