Sarlink® TPV R2 3180B by Teknor Apex is a high-durometer, resilient and multi-purpose thermoplastic vulcanizate (TPV) that contains 25% post-industrial recycled content. It helps to promote a circular economy while decreasing reliance on virgin fossil-based resources. It offers good adhesion, flexibility, moldability, processability, surface finish and weather resistance.
- Exhibits chemical resistance, heat aging resistance and medium hardness.
- It is suitable for injection molding, extrusion, overmolding, blow molding and co-extrusion with polypropylene or other thermoplastic elastomers (TPEs).
- It is used in automotive applications including exterior parts, interior parts and other under hood components.
- Sarlink® TPV R2 3180B is also recommended for agricultural applications, appliance components, seals, weatherstripping and industrial applications.
- Complies with RoHS.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Color | Visible After Login |
| Appearance | Visible After Login |
Compliance
| Certifications & Compliance | Visible After Login |
Applications
Recommended markets
Conversion mode
Availability
Product Status:Visible After Login
Regional Availability:Visible After Login| Visible After Login| Visible After Login
Sarlink® TPV R2 3180B properties
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Compression Set | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Compression Set | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Compression Set | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Shore A | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Shore A | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tear Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tear Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Stress at 100% Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Stress at 100% Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Stress at 100% Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Stress at 100% Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Specific Gravity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Sarlink® TPV R2 3180B Processing Guidelines
Extrusion Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Cylinder Zone 1 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 2 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 3 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 4 Temperature | Visible After Login | Visible After Login | |
| Die Temperature | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Take-Off Roll Temperature | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Back Pressure | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Front Temperature | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Middle Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Rear Temperature | Visible After Login | Visible After Login | |
| Screw Speed | Visible After Login | Visible After Login | |