LEXAN™ COPOLYMER EXL1112T (Americas)
Supplied bySABIC- Last Updated on Jun 18, 2024
LEXAN™ COPOLYMER EXL1112T (Americas) by SABIC is a general purpose, unfilled polycarbonate (PC) siloxane copolymer. It provides good low temperature (-20°C) ductility, high flow and excellent processability. It is a heat-stabilized grade offering high impact resistance and mold release with shorter cycle times compared to standard PC resins. It is available in wide range of transparent and opaque colors. Applications include electrical devices & displays, home appliances, electrical components & infrastructure, consumer, electrical and electronics. LEXAN™ COPOLYMER EXL1112T (Americas) is suitable for processing by injection molding.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Color | Visible After Login |
Documents related to LEXAN™ COPOLYMER EXL1112T (Americas)
Compliance
No data available
Applications
Recommended markets
Applications
Conversion mode
Availability
Product Status:Visible After Login
Regional Availability:Visible After Login| Visible After Login| Visible After Login
LEXAN™ COPOLYMER EXL1112T (Americas) properties
Electrical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Surface Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Volume Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame Rating, UL 94 | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Flammability Index (GWFI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Flammability Index (GWFI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Flammability Index (GWFI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Ignition Temperature (GWIT) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Ignition Temperature (GWIT) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Ignition Temperature (GWIT) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flexural Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Yield Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Rockwell L | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Dart Drop | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Optical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Haze | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Transmittance, Visible | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Transverse | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Volume Flow Rate (MVR) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Moisture Absorption | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption at Saturation | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| CTE, Linear, Parallel to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| CTE, Linear, Transverse to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Deflection Temperature at 1.8 MPa (264 psi) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| UL RTI, Electrical | 0.0 Visible After Login | Visible After Login | Visible After Login |
| UL RTI, Mechanical with Impact | 0.0 Visible After Login | Visible After Login | Visible After Login |
| UL RTI, Mechanical without Impact | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
LEXAN™ COPOLYMER EXL1112T (Americas) Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Back Pressure | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Drying Time (Cumulative) | Visible After Login | Visible After Login | |
| Front Zone 3 Temperature | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Middle Zone 2 Temperature | Visible After Login | Visible After Login | |
| Moisture Content | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Rear Zone 1 Temperature | Visible After Login | Visible After Login | |
| Screw Speed | Visible After Login | Visible After Login | |
| Shot to Cylinder Size | Visible After Login | Visible After Login | |