Technical datasheet
Zythane® 5070A
Supplied byAlliance Polymers & Services- Last Updated on Jun 27, 2024
Zythane® 5070A by Alliance Polymers & Services is polyester-based thermoplastic polyurethane (TPU) elastomer. It exhibits excellent abrasion resistance and toughness. This grade possesses good oil-, fuel-, & solvent resistance and good hydrolytic stability. Zythane® 5070A is processed by extrusion (blow molding) and injection molding (blow molding). It is used in spiral & pneumatic tubing, round & V-belting and blow molded bellows.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Appearance | Visible After Login |
Compliance
No data available
Applications
Recommended markets
No data available
Conversion mode
Availability
Product Status:Visible After Login
Zythane® 5070A properties
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame Rating, UL 94 | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Compression Set | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Compression Set | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Shore A | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tear Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Abrasion | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Abrasion | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Specific Gravity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Brittleness Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
Zythane® 5070A Processing Guidelines
Extrusion Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Cylinder Zone 1 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 2 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 3 Temperature | Visible After Login | Visible After Login | |
| Die Temperature | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Back Pressure | Visible After Login | Visible After Login | |
| Clamp Tonage | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Front Temperature | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Middle Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Rear Temperature | Visible After Login | Visible After Login | |
| Screw Speed | Visible After Login | Visible After Login | |