EDISTIR® N 2560 by Versalis (Eni Group) is a general-purpose, high molecular weight polystyrene (GPPS) grade. It exhibits improved elasticity, high stiffness, good mechanical strength, thermal resistance, and toughness. It is designed for thermoforming, sheet extrusion in blend with conventional & clear high impact polystyrene (HIPS) and for injection molding of complex items. It is suitable for food contact. It is recommended for thermoformed food packaging articles such as drink & dairy cups, plates, trays & for molded CD boxes, domestic appliances (refrigerators), stationery, cutlery, and housewares. EDISTIR® N 2560 complies with ISO 1622-PS, G, 095-03, EU No 10/2011 and UL 94 HB Flame Rating (UL file E83071).
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Color | Visible After Login |
| Appearance | Visible After Login |
Compliance
| Certifications & Compliance | Visible After Login |
Applications
Recommended markets
Applications
Conversion mode
Availability
Product Status:Visible After Login
EDISTIR® N 2560 properties
Electrical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Comparative Tracking Index (CTI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dielectric Constant | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dielectric Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dissipation Factor | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Surface Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Volume Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Auto-ignition Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flame Rating, UL 94 | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Test | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flexural Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Rockwell M | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density, Bulk | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| CTE, Linear, Parallel to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Heat Deflection Temperature (HDT), Annealed | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melting Point | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Thermal Conductivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
EDISTIR® N 2560 Processing Guidelines
Extrusion Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Melt Temperature | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Melt Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |