SYNTHOS PS GP 152 by Synthos Group is a colorless, general purpose polystyrene (GPPS) grade available in the form of cylindrical granules. It is modified by blending with the high-impact polystyrene (HIPS) and SBS copolymers. Exhibits excellent optical properties & gloss and increased heat resistance. Can be processed by injection molding, blow molding & co-extrusion and thermoforming. SYNTHOS PS GP 152 is recommended for packaging of cosmetics, CD & DVD cases, plates, vegetable boxes for refrigerators, biaxially-oriented sheets (BOPS) and shower enclosure panels.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Appearance | Visible After Login |
Compliance
No data available
Applications
Recommended markets
Applications
Conversion mode
Availability
Product Status:Visible After Login
SYNTHOS PS GP 152 properties
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame rating (UL 94) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Impact Strength, Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Styrene Residual Content | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
SYNTHOS PS GP 152 Processing Guidelines
Extrusion Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Melt Temperature | Visible After Login | Visible After Login | |
Extrusion/ Injection molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Drying Time (Hot-air Dryer) | Visible After Login | Visible After Login | |
| Drying Time (Molecular Sieve Dryer) | Visible After Login | Visible After Login | |
Extrusion/Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Melt Temperature | Visible After Login | Visible After Login | |