Technical datasheet
Enester® EM-555-GR5-V0-900
Supplied byRavago Manufacturing Americas- Last Updated on Jan 3, 2024
Enester® EM-555-GR5-V0-900 by Ravago Manufacturing Americas is a halogen-free, heat-stabilized polybutylene terephthalate grade reinforced with 30% glass fiber. It is suitable for processing by injection molding.
- It shows high lubrication, good mechanical and impact strength properties.
- Enester® EM-555-GR5-V0-900 is recommended for automotive applications.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
Compliance
No data available
Applications
Recommended markets
Conversion mode
Availability
Product Status:Visible After Login
Enester® EM-555-GR5-V0-900 properties
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame Rating, UL 94 | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Glow Wire Flammability Index (GWFI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Ash Content | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Deflection Temperature at 1.8 MPa (264 psi) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Enester® EM-555-GR5-V0-900 Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Zone 1 Temperature | Visible After Login | Visible After Login | |
| Zone 2 Temperature | Visible After Login | Visible After Login | |
| Zone 3 Temperature | Visible After Login | Visible After Login | |