PRE-ELEC® TP 11270 by Premix is a high density polyethylene (HDPE) grade. Is a conductive grade, achieved by using special conductive carbon black. Exhibits low electrical resistivity and excellent mechanical properties. PRE-ELEC® TP 11270 is recommended for manufacturing of automotive fuel system parts, extruded fuel filler pipes and injection molded fuel filler necks and heads.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Appearance | Visible After Login |
Compliance
No data available
Applications
Recommended markets
Conversion mode
Availability
Product Status:Visible After Login
PRE-ELEC® TP 11270 properties
Electrical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Surface Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Volume Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flexural Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Unnotched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Elongation | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Elongation | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Elongation | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Elongation | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Hardness, Shore | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Shore | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Specific Gravity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Heat Deflection Temperature (HDT) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Heat Deflection Temperature (HDT) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
PRE-ELEC® TP 11270 Processing Guidelines
Extrusion Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Cylinder Temperature (Zone 1) | Visible After Login | Visible After Login | |
| Cylinder Temperature (Zone 2) | Visible After Login | Visible After Login | |
| Cylinder Temperature (Zone 3) | Visible After Login | Visible After Login | |
| Cylinder Temperature (Zone 4) | Visible After Login | Visible After Login | |
| Cylinder Temperature (Zone 5) | Visible After Login | Visible After Login | |
| Cylinder Temperature (Zone 6) | Visible After Login | Visible After Login | |
| Die Temperature (Zone 1) | Visible After Login | Visible After Login | |
| Die Temperature (Zone 2) | Visible After Login | Visible After Login | |
| Die Temperature (Zone 3) | Visible After Login | Visible After Login | |
| Die Temperature (Zone 4) | Visible After Login | Visible After Login | |
| Die Temperature (Zone 5) | Visible After Login | Visible After Login | |
| Rolls Temperature (1st) | Visible After Login | Visible After Login | |
| Rolls Temperature (2nd) | Visible After Login | Visible After Login | |
| Rolls Temperature (3rd) | Visible After Login | Visible After Login | |
Extrusion/Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Pre-Drying Temperature | Visible After Login | Visible After Login | |
| Pre-drying Time | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Injection Pressure | Visible After Login | Visible After Login | |
| Injection Speed | Visible After Login | Visible After Login | |
| Material Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |