Technical datasheet
AKROMID® A28 GF 37 1 GIT black (5887)
Supplied byAkro-Plastic- Last Updated on Aug 27, 2025
AKROMID® A28 GF 37 1 GIT black (5887) by Akro-Plastic is 37% glass-fiber filled, heat stabilized, polyamide 66. AKROMID® A28 GF 37 1 GIT black (5887) exhibits easy flow with high stiffness & strength for gas injection technology. It is recommended for engineering parts. It is suitable for standard injection molding for good surface quality.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Color | Visible After Login |
Compliance
No data available
Applications
Recommended markets
Conversion mode
Availability
Product Status:Visible After Login
AKROMID® A28 GF 37 1 GIT black (5887) properties
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Burning Behavior | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Content Reinforcement | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Volume Flow Rate (MVR) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Melting Point | 0.0 Visible After Login | Visible After Login | Visible After Login |
AKROMID® A28 GF 37 1 GIT black (5887) Processing Guidelines
Injection Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Section 1 - Section 4 | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Back Pressure | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Feed Section | Visible After Login | Visible After Login | |
| Holding Pressure | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Moisture Content | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Screw Speed | Visible After Login | Visible After Login | |