GELOY™ Resin XP4034 by SABIC is an acrylic-styrene-acrylonitrile (ASA) +PC blend. Is an amorphous, durable grade with high gloss. Offers excellent weatherability, aesthetics and easy processability.
- Exhibits high heat-, impact and chemical resistance.
- Processed by injection molding/sheet extrusion or by co-extrusion/monolayer.
- GELOY™ Resin XP4034 recommended for unpainted exterior applications.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Color | Visible After Login |
Compliance
No data available
Applications
Recommended markets
No data available
Conversion mode
Availability
Product Status:Visible After Login
Regional Availability:Visible After Login| Visible After Login| Visible After Login
GELOY™ Resin XP4034 properties
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame rating (UL 94) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flame rating (UL 94) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Impact properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Instrumented Impact Total Energy | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Rockwell | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Optical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Gloss | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Elongation at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Specific Gravity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| CTE, Linear, Parallel to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| CTE, Linear, Transverse to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Heat Deflection Temperature (HDT) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Heat Deflection Temperature (HDT), Unannealed | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Heat Deflection Temperature (HDT), Unannealed | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Thermal Conductivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
GELOY™ Resin XP4034 Processing Guidelines
Extrusion Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Adapter Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 1 Temp. | Visible After Login | Visible After Login | |
| Cylinder Zone 2 Temp. | Visible After Login | Visible After Login | |
| Cylinder Zone 3 Temp. | Visible After Login | Visible After Login | |
| Cylinder Zone 4 Temp. | Visible After Login | Visible After Login | |
| Die Temperature | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Moisture Content | Visible After Login | Visible After Login | |
| Roll Stack Temp - Bottom | Visible After Login | Visible After Login | |
| Roll Stack Temp - Middle | Visible After Login | Visible After Login | |
| Roll Stack Temp - Top | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Back Pressure | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Drying Time (Cumulative) | Visible After Login | Visible After Login | |
| Front Temperature | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Middle Temperature | Visible After Login | Visible After Login | |
| Moisture Content (Max) | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Rear Temperature | Visible After Login | Visible After Login | |
| Shot to Cylinder Size | Visible After Login | Visible After Login | |
| Vent Depth | Visible After Login | Visible After Login | |