Ensoft SD-176-75A by Enplast is a styrenic block copolymer grade. It exhibits ozone- and UV resistance. Ensoft SD-176-75A by Enplast is suitable for processing by extrusion and injection molding.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
Compliance
No data available
Applications
Recommended markets
No data available
Conversion mode
Availability
Product Status:Visible After Login
Regional Availability:Visible After Login| Visible After Login| Visible After Login
Ensoft SD-176-75A properties
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| 100% Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| 300% Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Compression Set | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Compression Set | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Shore A | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tear Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Abrasion | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
Ensoft SD-176-75A Processing Guidelines
Extrusion Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Cylinder Zone 1 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 2 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 3 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 4 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 5 Temperature | Visible After Login | Visible After Login | |
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Melt Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
Injection molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Front Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Rear Temperature | Visible After Login | Visible After Login | |
| Screw Compression Ratio | Visible After Login | Visible After Login | |
| Screw L/D Ratio | Visible After Login | Visible After Login | |