Bayblend® T85 XF by Covestro is a polycarbonate (PC) and acrylonitrile butadiene styrene (ABS) blend. It is suitable for processing by injection molding. It has improved flow compared to T85. Bayblend® T85 XF complies with UL 94 HB flame rating.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
Compliance
No data available
Applications
Recommended markets
No data available
Conversion mode
Availability
Product Status:Visible After Login
Bayblend® T85 XF properties
Electrical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Comparative Tracking Index (CTI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dielectric Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dissipation Factor | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dissipation Factor | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Surface Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Volume Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame Rating, UL 94 | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Limiting Oxygen Index (LOI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Impact Strength, Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Stress at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Yield Strain | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Yield Stress | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Dielectric Constant | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Dielectric Constant | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Normal | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Volume Flow Rate (MVR) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Viscosity, Melt | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption at Equilibrium | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption at Saturation | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| CTE, Linear, Normal to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| CTE, Linear, Parallel to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Deflection Temperature at 0.46 MPa (66 psi) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Deflection Temperature at 1.8 MPa (264 psi) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
Bayblend® T85 XF Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Drying Temperature | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Moisture Content | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
Injection molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Barrel Front Temperature | Visible After Login | Visible After Login | |
| Barrel Middle Temperature | Visible After Login | Visible After Login | |
| Barrel Nozzle Temperature | Visible After Login | Visible After Login | |
| Barrel Rear Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Hold Pressure | Visible After Login | Visible After Login | |
| Injection Velocity | Visible After Login | Visible After Login | |
| Peripheral Screw Speed | Visible After Login | Visible After Login | |
| Plastic Back Pressure | Visible After Login | Visible After Login | |
| Shot-to-Cylinder Size | Visible After Login | Visible After Login | |
| Vent Depth | Visible After Login | Visible After Login | |