TARODUR 100 G3 is an acrylonitrile butadiene styrene (ABS) grade, reinforced with 17% glass fibers. Is a heat- and UV stabilized grade and contains antistatic additive. Exhibits low shrinkage, good dimensional stability and mechanical properties. Designed for injection molding process. Recommended for automotive applications. Complies with UNI EN ISO 9001:2008, ISO 9001:2008 Registration no., IT-3404, REACH Regulation (EC) No 1907/2006 and FIAT 55234 - 90.40 method.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Color | Visible After Login |
Compliance
| Certifications & Compliance | Visible After Login |
Applications
Recommended markets
Conversion mode
Availability
Product Status:Visible After Login
TARODUR 100 G3 properties
Electrical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Volume Resistivity | 0.0 Visible After Login | Visible After Login | Visible After Login |
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Glow Wire Flammability Index (GWFI) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Ball Pressure Test Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage, Transverse | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Water Absorption at Saturation | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| CTE, Linear, Parallel to Flow | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Heat Deflection Temperature (HDT), Unannealed | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Maximum Service Temperature, Air | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
TARODUR 100 G3 Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Drying Temperature | Visible After Login | Visible After Login | |
| Drying Time | Visible After Login | Visible After Login | |
| Melt Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Pre-Drying Temperature | Visible After Login | Visible After Login | |
| Pre-drying Time | Visible After Login | Visible After Login | |
| Rate of Injection | Visible After Login | Visible After Login | |