Luban RP2251T by Orpic is a nucleated polypropylene (PP) random copolymer. It is manufactured using the spheripol technology. It offers a very good flowability and an excellent transparency and organoleptic performance. It provides good adhesion with the inner barrier layer, without impacting the overall transparency and processability in multilayer barrier systems.
- It is suitable for processing by thin-wall injection molding.
- It has a superior aesthetic appearance and can be processed at significantly lower temperatures, enabling convertors to generate energy savings and improved productivity due to reduced cycle times.
- Luban RP2251T is recyclable and recommended for food packaging applications.
- It meets with the requirements of U.S FDA 21 CFR 177.1520.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
| Color | Visible After Login |
| Appearance | Visible After Login |
Compliance
| Food Contact Approval | Visible After Login |
| Certifications & Compliance | Visible After Login |
Applications
Recommended markets
Conversion mode
Availability
Product Status:Visible After Login
Luban RP2251T properties
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Elongation at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Elongation at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
Optical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Haze | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
Luban RP2251T Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Melt Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
Injection molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Hold Pressure | Visible After Login | Visible After Login | |