Denka HS-K190 by Denka is an alloy of acrylonitrile butadiene styrene (ABS) and polycarbonate (PC) resins.
- It is produced by using DENKA’s special compound technology and exhibits very high impact resistance.
- It can be processed by injection molding method.
- Denka HS-K190 is used in exterior parts of automobiles.
Product family:
Chemical family:
Product Type:
| Bio Based content | Visible After Login |
Compliance
| Certifications & Compliance | Visible After Login |
Applications
Recommended markets
Conversion mode
Availability
Product Status:Visible After Login
Denka HS-K190 properties
Flammability properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flame Rating, UL 94 | 0.0 Visible After Login | Visible After Login | Visible After Login |
Impact properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Impact Strength, Notched Charpy | 0.0 Visible After Login | Visible After Login | Visible After Login |
Mechanical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Flexural Modulus | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Flexural Strength | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Hardness, Rockwell R | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Impact Strength, Notched Izod | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Modulus of Elasticity | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Nominal Strain at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Tensile Strength at Break | 0.0 Visible After Login | Visible After Login | Visible After Login |
Other properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Tensile Strength at Yield | 0.0 Visible After Login | Visible After Login | Visible After Login |
Physical properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Density | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Linear Mold Shrinkage | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Melt Mass-Flow Rate (MFR or MFI = Melt Flow Index or MI = Melt Index) | 0.0 Visible After Login | Visible After Login | Visible After Login |
Thermal properties
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Deflection Temperature, Under Load at 1.8 MPa | 0.0 Visible After Login | Visible After Login | Visible After Login |
| Vicat Softening Temperature | 0.0 Visible After Login | Visible After Login | Visible After Login |
Denka HS-K190 Processing Guidelines
Injection Molding Processing Guidelines
| Properties | Value & unit | Test condition | Test method |
|---|---|---|---|
| Back Pressure | Visible After Login | Visible After Login | |
| Cylinder Zone 1 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 2 Temperature | Visible After Login | Visible After Login | |
| Cylinder Zone 3 Temperature | Visible After Login | Visible After Login | |
| Mold Temperature | Visible After Login | Visible After Login | |
| Nozzle Temperature | Visible After Login | Visible After Login | |
| Pre Drying Time | Visible After Login | Visible After Login | |
| Pre-Drying Temperature | Visible After Login | Visible After Login | |