Typical formulation ingredients

PHASEINGREDIENTSQuantitYActions
xVisible After Loginx%
xVisible After Loginx%
xVisible After Loginx%

End consumer benefits

No data available

Applications

Sub-applications

Application formats

No data available
No data available

Typical properties

Peel force, gms, after 14 days 85
Peel force, gms, after 1 month 80
Peel force, gms, after 24 hours 100
Peel force, gms, measured at 40°C on nonwoven after spiral spray application at 120° C6 101
Brookfield viscosity, cps, at 160° C 4000
Brookfield viscosity, cps, at 120° C 27000
Peel force, gms, measured at 40°C on nonwoven after spiral spray application at 140° C 88
Brookfield viscosity, cps, at 140° C 12500
Peel force, gms, measured at 40°C on nonwoven after spiral spray application at 120° C 100

Procedure

Visible After LoginVisible After Login Visible After Login-Visible After Login